Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.5 g/cm³ Show Supplier Material materials with Dichte of 1.5 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 10 GPa Show Supplier Material materials with Biegemodul of 10 GPa | dry | ISO 178 | |
Dehnung | 1.7 % Show Supplier Material materials with Dehnung of 1.7 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 11.5 GPa Show Supplier Material materials with Elastizitätsmodul of 11.5 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 4.6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.6 kJ/m² | dry | ISO 179/1eA |
Zugfestigkeit | 130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.7e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.7e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6.6e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 319 °C Show Supplier Material materials with Schmelzpunkt of 319 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 235 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 235 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | dry | IEC 60250 | 5GHz |
3.74 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.74 [-] | dry | IEC 60250 | 1GHz | |
3.75 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.75 [-] | conditioned | IEC 60250 | 5GHz | |
3.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-] | conditioned | IEC 60250 | 1GHz | |
Verlustfaktor | 109 [-] Show Supplier Material materials with Verlustfaktor of 109 [-] | dry | IEC 60250 | 5GHz |
137 [-] Show Supplier Material materials with Verlustfaktor of 137 [-] | dry | IEC 60250 | 1GHz | |
140 [-] Show Supplier Material materials with Verlustfaktor of 140 [-] | conditioned | IEC 60250 | 5GHz | |
170 [-] Show Supplier Material materials with Verlustfaktor of 170 [-] | conditioned | IEC 60250 | 1GHz |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 35% Glass Fiber |