Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.45 g/cm³ Show Supplier Material materials with Dichte of 1.45 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Wasserabsorption | 5.5 % Show Supplier Material materials with Wasserabsorption of 5.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 12 GPa Show Supplier Material materials with Biegemodul of 12 GPa | dry | ISO 178 | |
Dehnung | -40 °C | 3.1 % Show Supplier Material materials with Dehnung of 3.1 % | dry | ISO 527-1/-2 |
3.3 % Show Supplier Material materials with Dehnung of 3.3 % | dry | ISO 527-1/-2 | ||
6 % Show Supplier Material materials with Dehnung of 6 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 8 GPa Show Supplier Material materials with Elastizitätsmodul of 8 GPa | conditioned | ISO 527-1/-2 | |
13 GPa Show Supplier Material materials with Elastizitätsmodul of 13 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 315 MPa Show Supplier Material materials with Flexural yield strength of 315 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | dry | ISO 179/1eA |
-30 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | dry | ISO 179/1eA | |
23 °C | 22 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 22 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 85 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 85 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 95 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 95 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | -40 °C | 285 MPa Show Supplier Material materials with Zugfestigkeit of 285 MPa | dry | ISO 527-1/-2 |
140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | conditioned | ISO 527-1/-2 | ||
205 MPa Show Supplier Material materials with Zugfestigkeit of 205 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 2e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | 0.71 mm | UL746B | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperaturleitfähigkeit | 1.2e-07 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 1.2e-07 mm²/s | dry | - | |||
Vicat-Erweichungstemperatur | 215 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 215 °C | dry | ISO 306 | 50°C/h 50N | ||
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.4 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Dielektrizitätskonstante of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | conditioned | IEC 60243-1 | |
35 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 35 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 500 V Show Supplier Material materials with Kriechstromfestigkeit of 500 V | conditioned | IEC 60112 | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 50 [-] Show Supplier Material materials with Verlustfaktor of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Verlustfaktor of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
1100 [-] Show Supplier Material materials with Verlustfaktor of 1100 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Verlustfaktor of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1260 g/cm³ Show Supplier Material materials with Density of melt of 1260 g/cm³ | dry | - | |
Schrumpfung | 0.34 % Show Supplier Material materials with Schrumpfung of 0.34 % | dry | ISO 294-4 | Parallel |
0.83 % Show Supplier Material materials with Schrumpfung of 0.83 % | dry | ISO 294-4 | Normal | |
Specific heat capacity melt | 2080 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2080 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.32 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.32 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Airbag Containers, Front End Modules | |
Certifications | Yellow Card Available | |
Fillers | 40% Glass Fiber |