Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Bio-based content | 22 % Show Supplier Material materials with Bio-based content of 22 % | dry | ASTM D6866-12 Method B | |
Dichte | 1.23 g/cm³ Show Supplier Material materials with Dichte of 1.23 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.01 % Show Supplier Material materials with Moisture absorption of 0.01 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 0.15 % Show Supplier Material materials with Wasserabsorption of 0.15 % | dry | ISO 62 | at 23°C after 24h |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Biegemodul | 0.35 GPa Show Supplier Material materials with Biegemodul of 0.35 GPa | dry | ISO 178 | |
Dehnung | 105 % Show Supplier Material materials with Dehnung of 105 % | dry | ISO 527-1/-2 | |
640 % Show Supplier Material materials with Dehnung of 640 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.34 GPa Show Supplier Material materials with Elastizitätsmodul of 0.34 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 65 [-] Show Supplier Material materials with Härte, Shore D of 65 [-] | dry | ISO 868 | 3s |
Reißfestigkeit | 169 kN/m Show Supplier Material materials with Reißfestigkeit of 169 kN/m | dry | ISO 34-1; Method B | |
190 kN/m Show Supplier Material materials with Reißfestigkeit of 190 kN/m | dry | ISO 34-1; Method B | ||
Zugfestigkeit | 27 MPa Show Supplier Material materials with Zugfestigkeit of 27 MPa | dry | ISO 527-1/-2 | |
49 MPa Show Supplier Material materials with Zugfestigkeit of 49 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Glasübergangstemperatur | -2 °C Show Supplier Material materials with Glasübergangstemperatur of -2 °C | dry | ISO 11357-1/-2 | 10°C/min |
Schmelzpunkt | 210 °C Show Supplier Material materials with Schmelzpunkt of 210 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat-Erweichungstemperatur | 99 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 99 °C | dry | ISO 306 | 50°C/h 50N |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 5 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 5 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | ISO 294-4 | Parallel | |
1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | ||
1.75 % Show Supplier Material materials with Schrumpfung of 1.75 % | dry | ISO 294-4 | Normal | ||
1.75 % Show Supplier Material materials with Schrumpfung of 1.75 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Cooking Bag, Bio-based panliners, Snowboard Cover Laminates, Smokable Sausage Casings | |
Certifications | Food Contact |