Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.77 g/cm³ Show Supplier Material materials with Dichte of 1.77 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.3 % Show Supplier Material materials with Moisture absorption of 1.3 % | dry | Sim. to ISO 62 | |
Sauerstoffindex | 37 % Show Supplier Material materials with Sauerstoffindex of 37 % | dry | ISO 4589-1/-2 | |
Wasserabsorption | 1.3 % Show Supplier Material materials with Wasserabsorption of 1.3 % | dry | ISO 62 | at 23°C after 24h |
4.6 % Show Supplier Material materials with Wasserabsorption of 4.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Biegemodul | 10 GPa Show Supplier Material materials with Biegemodul of 10 GPa | conditioned | ISO 178 | |||
14 GPa Show Supplier Material materials with Biegemodul of 14 GPa | dry | ISO 178 | ||||
120 °C | 8.5 GPa Show Supplier Material materials with Biegemodul of 8.5 GPa | dry | ISO 178 | |||
160 °C | 5.5 GPa Show Supplier Material materials with Biegemodul of 5.5 GPa | dry | ISO 178 | |||
Dehnung | 1.8 % Show Supplier Material materials with Dehnung of 1.8 % | dry | ISO 527-1/-2 | 1 mm | ||
2 % Show Supplier Material materials with Dehnung of 2 % | dry | ISO 527-1/-2 | ||||
2.6 % Show Supplier Material materials with Dehnung of 2.6 % | conditioned | ISO 527-1/-2 | ||||
120 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | |||
160 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 11 GPa Show Supplier Material materials with Elastizitätsmodul of 11 GPa | conditioned | ISO 527-1/-2 | |||
16 GPa Show Supplier Material materials with Elastizitätsmodul of 16 GPa | dry | ISO 527-1/-2 | ||||
16 GPa Show Supplier Material materials with Elastizitätsmodul of 16 GPa | dry | ISO 527-1/-2 | 1 mm | |||
120 °C | 9.5 GPa Show Supplier Material materials with Elastizitätsmodul of 9.5 GPa | dry | ISO 527-1/-2 | |||
160 °C | 6.5 GPa Show Supplier Material materials with Elastizitätsmodul of 6.5 GPa | dry | ISO 527-1/-2 | |||
Flexural yield strength | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | conditioned | ISO 178 | |||
300 MPa Show Supplier Material materials with Flexural yield strength of 300 MPa | dry | ISO 178 | ||||
120 °C | 230 MPa Show Supplier Material materials with Flexural yield strength of 230 MPa | dry | ISO 178 | |||
160 °C | 200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | dry | ISO 178 | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | dry, conditioned | ISO 179/1eA | ||
23 °C | 14.0 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 14.0 kJ/m² | dry, conditioned | ISO 179/1eA | |||
Zugfestigkeit | 130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | conditioned | ISO 527-1/-2 | |||
200 MPa Show Supplier Material materials with Zugfestigkeit of 200 MPa | dry | ISO 527-1/-2 | ||||
200 MPa Show Supplier Material materials with Zugfestigkeit of 200 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
120 °C | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | dry | ISO 527-1/-2 | |||
160 °C | 90 MPa Show Supplier Material materials with Zugfestigkeit of 90 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 3 mm | IEC 60695-2-12 | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 0.75 mm | IEC 60695-2-12 | |||
Glow Wire Ignition Temperature | 825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | 0.75 mm | IEC 60695-2-13 | ||
960 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 960 °C | dry | 3 mm | IEC 60695-2-13 | |||
Koeffizient der thermischen Ausdehnung | 2.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Vicat-Erweichungstemperatur | 290 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 290 °C | dry | ISO 306 | 50°C/h 50N | ||
Wärmeformbeständigkeitstemperatur | 290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.6 [-] | dry | IEC 60250 | 1GHz |
3.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-] | conditioned | IEC 60250 | 1GHz | |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 1MHz | |
4.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.3 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
12 [-] Show Supplier Material materials with Dielektrizitätskonstante of 12 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 350 V Show Supplier Material materials with Kriechstromfestigkeit of 350 V | dry | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 60 [-] Show Supplier Material materials with Verlustfaktor of 60 [-] | dry | IEC 62631-2-1 | 100Hz |
160 [-] Show Supplier Material materials with Verlustfaktor of 160 [-] | dry | IEC 62631-2-1 | 1MHz | |
250 [-] Show Supplier Material materials with Verlustfaktor of 250 [-] | dry | IEC 60250 | 1GHz | |
325 [-] Show Supplier Material materials with Verlustfaktor of 325 [-] | conditioned | IEC 60250 | 1GHz | |
700 [-] Show Supplier Material materials with Verlustfaktor of 700 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3300 [-] Show Supplier Material materials with Verlustfaktor of 3300 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+08 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+08 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | dry | Sim. to ISO 294-4 | Parallel |
0.9 % Show Supplier Material materials with Schrumpfung of 0.9 % | dry | Sim. to ISO 294-4 | Normal | |
Spiral flow length | 110 | dry | - | 1.0 mm 800 bar |
120 | dry | - | 1.0 mm 900 bar | |
130 | dry | - | 1.0 mm 1000 bar | |
Viscosity number | 150 cm³/gr Show Supplier Material materials with Viscosity number of 150 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Reflow connectors, FPC connectors, WtB and BtB Connectors, Relay Bases | |
Certifications | Yellow Card Available | |
Fillers | 40% Glass Fiber |