Allgemein
Property | Value |
---|---|
Relative Dichte | 8.78 [-] Show Supplier Material materials with Relative Dichte of 8.78 [-] |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefähigkeit 90°, in longitudinaler Richtung | 0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0 [-] | EH Temper | |
0.8 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0.8 [-] | SH Temper | |
1.6 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 1.6 [-] | ESH Temper | |
2.5 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 2.5 [-] | XSH Temper | |
Biegefähigkeit 90°, in transversaler Richtung | 0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 0 [-] | H Temper |
1.5 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 1.5 [-] | EH Temper | |
2 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 2 [-] | SH Temper | |
3.3 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 3.3 [-] | ESH Temper | |
Biegemodul | 100 GPa Show Supplier Material materials with Biegemodul of 100 GPa | |
Dehnung | 2 % Show Supplier Material materials with Dehnung of 2 % | XSH Temper |
2.4 % Show Supplier Material materials with Dehnung of 2.4 % | ESH Temper | |
9.2 % Show Supplier Material materials with Dehnung of 9.2 % | SH Temper | |
15.3 % Show Supplier Material materials with Dehnung of 15.3 % | EH Temper | |
25.6 % Show Supplier Material materials with Dehnung of 25.6 % | H Temper | |
Elastizitätsmodul | 105 GPa Show Supplier Material materials with Elastizitätsmodul of 105 GPa | |
Härte, Vickers | 223 [-] Show Supplier Material materials with Härte, Vickers of 223 [-] | H Temper |
245 [-] Show Supplier Material materials with Härte, Vickers of 245 [-] | EH Temper | |
267 [-] Show Supplier Material materials with Härte, Vickers of 267 [-] | SH Temper | |
285 [-] Show Supplier Material materials with Härte, Vickers of 285 [-] | ESH Temper | |
305 [-] Show Supplier Material materials with Härte, Vickers of 305 [-] | XSH Temper | |
Streckgrenze | 558 MPa Show Supplier Material materials with Streckgrenze of 558 MPa | H Temper | for spring material (Kb0.1) |
585 MPa Show Supplier Material materials with Streckgrenze of 585 MPa | EH Temper | for spring material (Kb0.1) | |
657 MPa Show Supplier Material materials with Streckgrenze of 657 MPa | H Temper, RP02 | |
661 MPa Show Supplier Material materials with Streckgrenze of 661 MPa | SH Temper | for spring material (Kb0.1) | |
718 MPa Show Supplier Material materials with Streckgrenze of 718 MPa | ESH Temper | for spring material (Kb0.1) | |
783 MPa Show Supplier Material materials with Streckgrenze of 783 MPa | EH Temper, RP02 | |
877 MPa Show Supplier Material materials with Streckgrenze of 877 MPa | SH Temper, RP02 | |
883 MPa Show Supplier Material materials with Streckgrenze of 883 MPa | XSH Temper | for spring material (Kb0.1) | |
988 MPa Show Supplier Material materials with Streckgrenze of 988 MPa | ESH Temper, RP02 | |
1044 MPa Show Supplier Material materials with Streckgrenze of 1044 MPa | XSH Temper, RP02 | |
Zugfestigkeit | 693 MPa Show Supplier Material materials with Zugfestigkeit of 693 MPa | H Temper |
800 MPa Show Supplier Material materials with Zugfestigkeit of 800 MPa | EH Temper | |
890 MPa Show Supplier Material materials with Zugfestigkeit of 890 MPa | SH Temper | |
1000 MPa Show Supplier Material materials with Zugfestigkeit of 1000 MPa | ESH Temper | |
1058 MPa Show Supplier Material materials with Zugfestigkeit of 1058 MPa | XSH Temper |
Thermisch
Property | Value |
---|---|
Koeffizient der thermischen Ausdehnung | 1.84e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.84e-05 1/K |
Schmelzpunkt | 845 - 1000 °C Show Supplier Material materials with Schmelzpunkt of 845 - 1000 °C |
Spezifische Wärmekapazität | 375 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 375 J/(kg·K) |
Wärmeleitfähigkeit | 50 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 50 W/(m·K) |
Elektrisch
Property | Value |
---|---|
Specific Electrical conductivity | 10 % IACS Show Supplier Material materials with Specific Electrical conductivity of 10 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Andere | 99.8 % Show Supplier Material materials with Andere of 99.8 % | min. | Cu+Sn+P |
Blei | 0.01 % Show Supplier Material materials with Blei of 0.01 % | max. |
Eisen | 0.01 % Show Supplier Material materials with Eisen of 0.01 % | max. |
Phosphor | 0.04 - 0.2 % Show Supplier Material materials with Phosphor of 0.04 - 0.2 % | |
Zink | 0.01 % Show Supplier Material materials with Zink of 0.01 % | max. |
Zinn | 9 - 11 % Show Supplier Material materials with Zinn of 9 - 11 % |
Technological properties
Property | ||
---|---|---|
Application areas | The grade is particularly suitable for electronics (connectors, lead frames, lead terminals, transistor terminals, etc.), electrical (relay and switch contacts, rotary switch slides and contacts, fuse clips, etc.), automotive (bearing frames, hydraulic equipment caps, packing, bearings, clutch disks, electrical parts, etc.) and others (bellows, slides, blades, plate springs, corrosion-proof machinery equipment, diaphragms, etc.) | |
Coating | Standard product specification of a HOT-DIP-tinned strip. *Width means the slit width after plating. *Different plating thickness for each side is possible. * We can accommodate our products to individual specifications other than the above standard specifications. Please feel free to call us. | |
Other | Please contact the supplier if you have any specific requests regarding chemical compostions, mechanical properties, and thickness. | |
Tolerances |