Allgemein
Property | Value |
---|---|
Relative Dichte | 8.8 [-] Show Supplier Material materials with Relative Dichte of 8.8 [-] |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefähigkeit 90°, in longitudinaler Richtung | 0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0 [-] | EH Temper | |
0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0 [-] | SH Temper | |
0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0 [-] | ESH Temper | |
0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0 [-] | XSH Temper | |
Biegefähigkeit 90°, in transversaler Richtung | 0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 0 [-] | EH Temper | |
0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 0 [-] | SH Temper | |
2 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 2 [-] | ESH Temper | |
4 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 4 [-] | XSH Temper | |
Biegemodul | 100 GPa Show Supplier Material materials with Biegemodul of 100 GPa | |
Dehnung | 2.1 % Show Supplier Material materials with Dehnung of 2.1 % | XSH Temper |
9.3 % Show Supplier Material materials with Dehnung of 9.3 % | ESH Temper | |
13.3 % Show Supplier Material materials with Dehnung of 13.3 % | SH Temper | |
23.2 % Show Supplier Material materials with Dehnung of 23.2 % | EH Temper | |
35.3 % Show Supplier Material materials with Dehnung of 35.3 % | H Temper | |
Elastizitätsmodul | 110 GPa Show Supplier Material materials with Elastizitätsmodul of 110 GPa | |
Härte, Vickers | 197 [-] Show Supplier Material materials with Härte, Vickers of 197 [-] | H Temper |
229 [-] Show Supplier Material materials with Härte, Vickers of 229 [-] | EH Temper | |
242 [-] Show Supplier Material materials with Härte, Vickers of 242 [-] | SH Temper | |
258 [-] Show Supplier Material materials with Härte, Vickers of 258 [-] | ESH Temper | |
285 [-] Show Supplier Material materials with Härte, Vickers of 285 [-] | XSH Temper | |
Streckgrenze | 469 MPa Show Supplier Material materials with Streckgrenze of 469 MPa | H Temper | for spring material (Kb0.1) |
563 MPa Show Supplier Material materials with Streckgrenze of 563 MPa | EH Temper | for spring material (Kb0.1) | |
569 MPa Show Supplier Material materials with Streckgrenze of 569 MPa | H Temper, RP02 | |
632 MPa Show Supplier Material materials with Streckgrenze of 632 MPa | SH Temper | for spring material (Kb0.1) | |
648 MPa Show Supplier Material materials with Streckgrenze of 648 MPa | ESH Temper | for spring material (Kb0.1) | |
694 MPa Show Supplier Material materials with Streckgrenze of 694 MPa | EH Temper, RP02 | |
706 MPa Show Supplier Material materials with Streckgrenze of 706 MPa | XSH Temper | for spring material (Kb0.1) | |
773 MPa Show Supplier Material materials with Streckgrenze of 773 MPa | SH Temper, RP02 | |
834 MPa Show Supplier Material materials with Streckgrenze of 834 MPa | ESH Temper, RP02 | |
968 MPa Show Supplier Material materials with Streckgrenze of 968 MPa | XSH Temper, RP02 | |
Zugfestigkeit | 616 MPa Show Supplier Material materials with Zugfestigkeit of 616 MPa | H Temper |
721 MPa Show Supplier Material materials with Zugfestigkeit of 721 MPa | EH Temper | |
778 MPa Show Supplier Material materials with Zugfestigkeit of 778 MPa | SH Temper | |
845 MPa Show Supplier Material materials with Zugfestigkeit of 845 MPa | ESH Temper | |
979 MPa Show Supplier Material materials with Zugfestigkeit of 979 MPa | XSH Temper |
Thermisch
Property | Value |
---|---|
Koeffizient der thermischen Ausdehnung | 1.82e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.82e-05 1/K |
Schmelzpunkt | 880 - 1020 °C Show Supplier Material materials with Schmelzpunkt of 880 - 1020 °C |
Spezifische Wärmekapazität | 377 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) |
Wärmeleitfähigkeit | 63 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 63 W/(m·K) |
Elektrisch
Property | Value |
---|---|
Specific Electrical conductivity | 12 % IACS Show Supplier Material materials with Specific Electrical conductivity of 12 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Andere | 99.8 % Show Supplier Material materials with Andere of 99.8 % | min. | Cu+Sn+P |
Blei | 0.01 % Show Supplier Material materials with Blei of 0.01 % | max. |
Eisen | 0.01 % Show Supplier Material materials with Eisen of 0.01 % | max. |
Phosphor | 0.03 - 0.2 % Show Supplier Material materials with Phosphor of 0.03 - 0.2 % | |
Zink | 0.01 % Show Supplier Material materials with Zink of 0.01 % | max. |
Zinn | 7 - 9 % Show Supplier Material materials with Zinn of 7 - 9 % |
Technological properties
Property | ||
---|---|---|
Application areas | The grade is particularly suitable for electronics (connectors, lead frames, lead terminals, transistor terminals, etc.), electrical (relay and switch contacts, rotary switch slides and contacts, fuse clips, etc.), automotive (bearing frames, hydraulic equipment caps, packing, bearings, clutch disks, electrical parts, etc.) and others (bellows, slides, blades, plate springs, corrosion-proof machinery equipment, diaphragms, etc.) | |
Coating | Standard product specification of a HOT-DIP-tinned strip. *Width means the slit width after plating. *Different plating thickness for each side is possible. * We can accommodate our products to individual specifications other than the above standard specifications. Please feel free to call us. | |
Other | Please contact the supplier if you have any specific requests regarding chemical compostions, mechanical properties, and thickness. | |
Tolerances |