Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.48 g/cm³ Show Supplier Material materials with Dichte of 4.48 g/cm³ |
Mechanisch
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 1700 °C Show Supplier Material materials with Schmelzpunkt of 1700 °C | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 2.5 - 3.5 % Show Supplier Material materials with Aluminium of 2.5 - 3.5 % | ||
Andere | 0.04 % Show Supplier Material materials with Andere of 0.04 % | max. | |
Eisen | 0.25 % Show Supplier Material materials with Eisen of 0.25 % | max. | |
Nickel | 0.03 % Show Supplier Material materials with Nickel of 0.03 % | max. | |
Sauerstoff | 0.15 % Show Supplier Material materials with Sauerstoff of 0.15 % | max. | |
Stickstoff | 0.05 % Show Supplier Material materials with Stickstoff of 0.05 % | max. | |
Titan | Balance | ||
Vanadium | 2 - 3 % Show Supplier Material materials with Vanadium of 2 - 3 % | ||
Wasserstoff | 0.02 % Show Supplier Material materials with Wasserstoff of 0.02 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Used in aircraft applications where strength is required but weight is a critical factor. Ti-3Al-2.5V is used in tubular form since it has proven to be much more malleable than Ti-6-4 and has useful properties for applications in hydraulic systems. Ti-3Al-2.5V titanium tubing can be cold worked by standard tube manufacturing processes or supplied in the annealed condition. Other applications include, bicycle and wheel chairs frames. | |
Corrosion properties | Excellent Resistance to pitting and crevice / erosion corrosion |