Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 18.8 g/cm³ Show Supplier Material materials with Dichte of 18.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 20 % Show Supplier Material materials with Dehnung of 20 % | min. |
Elastizitätsmodul | 23.0 °C | 180 GPa Show Supplier Material materials with Elastizitätsmodul of 180 GPa | |
Härte, Vickers | 23.0 °C | 220 - 230 [-] Show Supplier Material materials with Härte, Vickers of 220 - 230 [-] | |
Schubmodule | 23.0 °C | 74 GPa Show Supplier Material materials with Schubmodule of 74 GPa | |
Streckgrenze Rp 0,2 | 23.0 °C | 410 - 460 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 410 - 460 MPa | |
Zugfestigkeit | 23.0 °C | 620 - 710 MPa Show Supplier Material materials with Zugfestigkeit of 620 - 710 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.02E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.02E-5 1/K | RT-100 °C |
Schmelzpunkt | 1660 - 1700 °C Show Supplier Material materials with Schmelzpunkt of 1660 - 1700 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Specific Electrical conductivity | 5.6 - 5.77 % IACS Show Supplier Material materials with Specific Electrical conductivity of 5.6 - 5.77 % IACS | ||
Temperaturwiderstandskoeffizient | 23.0 °C | 1.25E-3 - 1.35E-3 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 1.25E-3 - 1.35E-3 1/K | 0-100 °C |
spezifischer Widerstand | 23.0 °C | 2.98E-7 - 3.04E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.98E-7 - 3.04E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Spark plugs, electrodes | |
Corrosion properties | Corrosion resistant | |
Other | Ductile |