Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 20 g/cm³ Show Supplier Material materials with Dichte of 20 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 38 % Show Supplier Material materials with Dehnung of 38 % | |
1200.0 °C | 42 % Show Supplier Material materials with Dehnung of 42 % | ||
1400.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % | ||
1600.0 °C | 54 % Show Supplier Material materials with Dehnung of 54 % | ||
Elastizitätsmodul | 23.0 °C | 213 GPa Show Supplier Material materials with Elastizitätsmodul of 213 GPa | |
Härte, Vickers | 23.0 °C | 94 [-] Show Supplier Material materials with Härte, Vickers of 94 [-] | |
Kriechfestigkeit | 1200.0 °C | 2.4 MPa Show Supplier Material materials with Kriechfestigkeit of 2.4 MPa | 10,000 h (extrapolated data) |
1400.0 °C | 1.3 MPa Show Supplier Material materials with Kriechfestigkeit of 1.3 MPa | 10,000 h (extrapolated data) | |
1600.0 °C | 0.5 MPa Show Supplier Material materials with Kriechfestigkeit of 0.5 MPa | 10,000 h (extrapolated data) | |
Norton Exponent | 1200.0 °C | 3.6 [-] Show Supplier Material materials with Norton Exponent of 3.6 [-] | |
1400.0 °C | 3.6 [-] Show Supplier Material materials with Norton Exponent of 3.6 [-] | ||
1600.0 °C | 3.8 [-] Show Supplier Material materials with Norton Exponent of 3.8 [-] | ||
Streckgrenze Rp 0,2 | 20.0 °C | 134 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 134 MPa | |
1200.0 °C | 44.3 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 44.3 MPa | ||
1400.0 °C | 27.7 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 27.7 MPa | ||
1600.0 °C | 14.7 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 14.7 MPa | ||
Zugfestigkeit | 20.0 °C | 301 MPa Show Supplier Material materials with Zugfestigkeit of 301 MPa | |
1200.0 °C | 58.8 MPa Show Supplier Material materials with Zugfestigkeit of 58.8 MPa | ||
1400.0 °C | 35.4 MPa Show Supplier Material materials with Zugfestigkeit of 35.4 MPa | ||
1600.0 °C | 16.7 MPa Show Supplier Material materials with Zugfestigkeit of 16.7 MPa | ||
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 1840 - 1870 °C Show Supplier Material materials with Schmelzpunkt of 1840 - 1870 °C | |
Wärmeleitfähigkeit | 20.0 °C | 40.1 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 40.1 W/(m·K) |
1200.0 °C | 70.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 70.6 W/(m·K) | |
1400.0 °C | 70.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 70.8 W/(m·K) | |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 2.1E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.1E-7 Ω·m |
1153.0 °C | 5.3E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.3E-7 Ω·m | |
1400.0 °C | 5.9E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.9E-7 Ω·m | |