Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 21.45 g/cm³ Show Supplier Material materials with Dichte of 21.45 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 23 % Show Supplier Material materials with Dehnung of 23 % |
1200.0 °C | 64 % Show Supplier Material materials with Dehnung of 64 % | |
1400.0 °C | 68 % Show Supplier Material materials with Dehnung of 68 % | |
1600.0 °C | 64 % Show Supplier Material materials with Dehnung of 64 % | |
Elastizitätsmodul | 20.0 °C | 165 GPa Show Supplier Material materials with Elastizitätsmodul of 165 GPa |
1600.0 °C | 60 GPa Show Supplier Material materials with Elastizitätsmodul of 60 GPa | |
Härte, Vickers | 23.0 °C | 42 [-] Show Supplier Material materials with Härte, Vickers of 42 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 59 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 59 MPa |
1200.0 °C | 7.6 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 7.6 MPa | |
1400.0 °C | 3.9 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 3.9 MPa | |
1600.0 °C | 3 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 3 MPa | |
Zugfestigkeit | 20.0 °C | 128 MPa Show Supplier Material materials with Zugfestigkeit of 128 MPa |
1200.0 °C | 15.6 MPa Show Supplier Material materials with Zugfestigkeit of 15.6 MPa | |
1400.0 °C | 8.2 MPa Show Supplier Material materials with Zugfestigkeit of 8.2 MPa | |
1600.0 °C | 4.4 MPa Show Supplier Material materials with Zugfestigkeit of 4.4 MPa | |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 1769 °C Show Supplier Material materials with Schmelzpunkt of 1769 °C | |
Wärmeleitfähigkeit | 20.0 °C | 69.11 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 69.11 W/(m·K) |
1200.0 °C | 88.02 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 88.02 W/(m·K) | |
1400.0 °C | 90.59 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 90.59 W/(m·K) | |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 9.83E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 9.83E-8 Ω·m |
1200.0 °C | 4.85E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.85E-7 Ω·m | |
1400.0 °C | 5.33E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.33E-7 Ω·m | |