Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 21.54 g/cm³ Show Supplier Material materials with Dichte of 21.54 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 215 GPa Show Supplier Material materials with Elastizitätsmodul of 215 GPa |
Härte, Vickers | 23.0 °C | 210 - 220 [-] Show Supplier Material materials with Härte, Vickers of 210 - 220 [-] |
Schubmodule | 23.0 °C | 72 GPa Show Supplier Material materials with Schubmodule of 72 GPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.7E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.7E-6 1/K | up to 300°C |
Schmelzpunkt | 1780 - 1800 °C Show Supplier Material materials with Schmelzpunkt of 1780 - 1800 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Specific Electrical conductivity | 6.8 - 7.02 % IACS Show Supplier Material materials with Specific Electrical conductivity of 6.8 - 7.02 % IACS | ||
Temperaturwiderstandskoeffizient | 23.0 °C | 1.21E-3 - 1.26E-3 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 1.21E-3 - 1.26E-3 1/K | 0-100 °C |
spezifischer Widerstand | 23.0 °C | 2.45E-7 - 2.52E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.45E-7 - 2.52E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Spark plugs, electrodes, thermocouples | |
Corrosion properties | Corrosion resistant | |
Other | Ductile, Biocompatible |