Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 13.2 % Show Material materials with Dehnung of 13.2 % | Predicted Value, A200 | ||||
13.3 % Show Material materials with Dehnung of 13.3 % | Predicted Value, Transverse | |||||
17.7 % Show Material materials with Dehnung of 17.7 % | Predicted Value, A80 Transverse | |||||
18.6 % Show Material materials with Dehnung of 18.6 % | Predicted Value, A5 | |||||
18.6 % Show Material materials with Dehnung of 18.6 % | Predicted Value, A50 | |||||
20 °C | 11 % Show Material materials with Dehnung of 11 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 11 % Show Material materials with Dehnung of 11 % | thermomechanically rolled | EN 10149-2 | Flat | ||
20 °C | 13 % Show Material materials with Dehnung of 13 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 13 % Show Material materials with Dehnung of 13 % | thermomechanically rolled | EN 10149-2 | Flat | ||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||||
Flächenreduzierung | 39.6 % Show Material materials with Flächenreduzierung of 39.6 % | Predicted Value | ||||
44.2 % Show Material materials with Flächenreduzierung of 44.2 % | Predicted Value, Transverse | |||||
Härte, Brinell | 249 [-] Show Material materials with Härte, Brinell of 249 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Scherfestigkeit | 571.7 MPa Show Material materials with Scherfestigkeit of 571.7 MPa | Predicted Value | ||||
Schubmodule | 80.2 GPa Show Material materials with Schubmodule of 80.2 GPa | Predicted Value | ||||
Streckgrenze | 288.4 MPa Show Material materials with Streckgrenze of 288.4 MPa | Predicted Value, RP1 | ||||
328.2 MPa Show Material materials with Streckgrenze of 328.2 MPa | Predicted Value, RP1 Transverse | |||||
493.8 MPa Show Material materials with Streckgrenze of 493.8 MPa | Predicted Value, Transverse | |||||
501.6 MPa Show Material materials with Streckgrenze of 501.6 MPa | Predicted Value, RP02 Transverse | |||||
524.2 MPa Show Material materials with Streckgrenze of 524.2 MPa | Predicted Value, RP02 | |||||
547.5 MPa Show Material materials with Streckgrenze of 547.5 MPa | Predicted Value, RP05 | |||||
619.8 MPa Show Material materials with Streckgrenze of 619.8 MPa | Predicted Value, RP002 | |||||
20 °C | 600 MPa Show Material materials with Streckgrenze of 600 MPa | thermomechanically rolled | EN 10149-2 | Flat | ||
Zugfestigkeit | 20 °C | 650 - 820 MPa Show Material materials with Zugfestigkeit of 650 - 820 MPa | thermomechanically rolled | EN 10149-2 | Flat |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.98 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.98 1/K | Predicted Value |
Spezifische Wärmekapazität | 453.5 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 453.5 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 37.81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 37.81 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.015 % Show Material materials with Aluminium of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Bor | 0.005 % Show Material materials with Bor of 0.005 % | thermomechanically rolled | EN 10149-2 | Flat |
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % | thermomechanically rolled | EN 10149-2 | Flat |
Mangan | 1.9 % Show Material materials with Mangan of 1.9 % | thermomechanically rolled | EN 10149-2 | Flat |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % | thermomechanically rolled | EN 10149-2 | Flat |
Niobium | 0.09 % Show Material materials with Niobium of 0.09 % | thermomechanically rolled | EN 10149-2 | Flat |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | thermomechanically rolled | EN 10149-2 | Flat |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | thermomechanically rolled | EN 10149-2 | Flat |
Titan | 0.22 % Show Material materials with Titan of 0.22 % | thermomechanically rolled | EN 10149-2 | Flat |
Vanadium | 0.2 % Show Material materials with Vanadium of 0.2 % | thermomechanically rolled | EN 10149-2 | Flat |