Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Dichte of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 11 - 16 % Show Material materials with Dehnung A50 of 11 - 16 % | |
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel |
Flächenreduzierung | 23.0 °C | 30 - 50 % Show Material materials with Flächenreduzierung of 30 - 50 % | |
Härte, Brinell | 23.0 °C | 277 [-] Show Material materials with Härte, Brinell of 277 [-] | |
Härte, Rockwell C | 23.0 °C | 28 [-] Show Material materials with Härte, Rockwell C of 28 [-] | |
Kerbschlagenergie | 23.0 °C | 27 - 41 J Show Material materials with Kerbschlagenergie of 27 - 41 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Martensitic Stainless Steel |
Streckgrenze | 23.0 °C | 725 MPa Show Material materials with Streckgrenze of 725 MPa | |
Zugfestigkeit | 23.0 °C | 930 MPa Show Material materials with Zugfestigkeit of 930 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Schmelzpunkt | 1370 - 1530 °C Show Material materials with Schmelzpunkt of 1370 - 1530 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 14 - 15.5 % Show Material materials with Chrom of 14 - 15.5 % |
Kohlenstoff | 0.07 % Show Material materials with Kohlenstoff of 0.07 % |
Kupfer | 2.5 - 4.5 % Show Material materials with Kupfer of 2.5 - 4.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 3.5 - 5.5 % Show Material materials with Nickel of 3.5 - 5.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |