EN 10292 Grade HX300BD hot rolled or cold rolled, hot dip coated,+Z, +ZF, +ZA, +AZ, +AS

View suppliers (3)
Want to keep this datasheet? Save it now in your required format

Description

The steel HX300BD (X=roll condition, B=bake hardening, D=hot-dip coatable) is producible with the following coatings: - HX300BD+Z (plating Zn) with coating weights (double-sided) of 100, 140, 200, 225 and 275 g/m² (100 g approximate 7,1 µm per side) - HX300BD+ZF (plating Zn-Fe) with coating weights (double-sided) of 100 and 120 g/m² (100 g approximate 7,1 µm per side) - HX300BD+ZA (plating Zn-Al) with coating weights (double-sided) of 095, 130, 185, 200 and 255 g/m² (95 g approximate 7,2 µm per side) - HX300BD+AZ (plating Al-Zn) with coating weights (double-sided) of 100, 150 and 185 g/m² (100 g approximate 13,3 µm per side) - HX300BD+AS (plating Al-Si) with coating weights (double-sided) of 060 and 080 g/m² (100 g approximate 17 µm per side) The hot dip galvanizing refined flat products are available by arrangement on ordering with different coating weights (also per side). Following surface protection types can be delivered: chemical passivated, oiled, chemical passivated and oiled, sealed, phosphated, phosphated and oiled. Mechanical properties are warranted for a period of 3 months for Bake-hardening steels and for a period of 6 months after provision of the products for all other sorts. The same terms are valid for freedom from stretcher strains (surface type B and C). It is suitable for usual welding methods. For higher coating weights on welding are where approppriate necessary special measures. Furthermore suitability for joining by sticking as well as for application of organic coatings. Application: household appliances industry, construction trade, electrical industry, furniture industry, car industry.,The steel HX300BD (X=roll condition, B=bake hardening, D=hot-dip coatable) is deliverable with the following coatings: - HX300BD+Z (plating Zn) with coating weights (double-sided) of 100, 140, 200, 225 and 275 g/m² (100 g approximate 7,1 µm per side) - HX300BD+ZF (plating Zn-Fe) with coating weights (double-sided) of 100 and 120 g/m² (100 g approximate 7,1 µm per side) - HX300BD+ZA (plating Zn-Al) with coating weights (double-sided) of 095, 130, 185, 200 and 255 g/m² (95 g approximate 7,2 µm per side) - HX300BD+AZ (plating Al-Zn) with coating weights (double-sided) of 100, 150 and 185 g/m² (100 g approximate 13,3 µm per side) - HX300BD+AS (plating Al-Si) with coating weights (double-sided) of 060 and 080 g/m² (100 g approximate 17 µm per side) The hot dip galvanizing refined flat products are available by arrangement on ordering with different coating weights (also per side). Following surface protection types can be delivered: chemical passivated, oiled, chemical passivated and oiled, sealed, phosphated, phosphated and oiled. Mechanical properties are warranted for a period of 3 months after provision. The same time is valid for freedom from stretcher strains (surface type B and C). It is suitable for usual welding methods. For higher coating weights on welding are where approppriate necessary special measures. Furthermore suitability for joining by sticking as well as for application of organic coatings. Application: household appliances industry, construction trade, electrical industry, furniture industry, car industry.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Dichte

20.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Dichte of 7.8 - 7.9 g/cm³

Typical for Manganese Steel

Mechanisch

PropertyTemperatureValueComment

Dehnung A80, transversal

20.0 °C

26 %

Show Material materials with Dehnung A80, transversal of 26 %

Elastizitätsmodul

20.0 °C

200 - 215 GPa

Show Material materials with Elastizitätsmodul of 200 - 215 GPa

Typical for Manganese Steel

Poissonzahl

20.0 °C

0.29 [-]

Show Material materials with Poissonzahl of 0.29 [-]

Typical for Manganese Steel

Streckgrenze Rp 0,2, transversal

20.0 °C

300 - 360 MPa

Show Material materials with Streckgrenze Rp 0,2, transversal of 300 - 360 MPa

Zugfestigkeit, transversal

20.0 °C

400 - 480 MPa

Show Material materials with Zugfestigkeit, transversal of 400 - 480 MPa

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

20.0 °C

1.33E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.33E-5 1/K

Typical for Manganese Steel

Schmelzpunkt

1382 - 1529 °C

Show Material materials with Schmelzpunkt of 1382 - 1529 °C

Typical for Manganese Steel

Spezifische Wärmekapazität

20.0 °C

510 - 553 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 510 - 553 J/(kg·K)

Typical for Manganese Steel

Wärmeleitfähigkeit

20.0 °C

14 - 16 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 14 - 16 W/(m·K)

Typical for Manganese Steel

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Kohlenstoff

0.11 %

Show Material materials with Kohlenstoff of 0.11 %

Mangan

0.7 - 0.8 %

Show Material materials with Mangan of 0.7 - 0.8 %

Niobium

0.09 %

Show Material materials with Niobium of 0.09 %

Phosphor

0.12 %

Show Material materials with Phosphor of 0.12 %

Schwefel

0.025 %

Show Material materials with Schwefel of 0.025 %

Silizium

0.5 %

Show Material materials with Silizium of 0.5 %

Titan

0.12 %

Show Material materials with Titan of 0.12 %