Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 14 % Show Material materials with Dehnung of 14 % | |
Elastizitätsmodul | 23.0 °C | 210 GPa Show Material materials with Elastizitätsmodul of 210 GPa | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for High Carbon Steel |
Schubmodule | 23.0 °C | 81 GPa Show Material materials with Schubmodule of 81 GPa | Typical for High Carbon Steel |
Streckgrenze | 23.0 °C | 460 MPa Show Material materials with Streckgrenze of 460 MPa | |
Zugfestigkeit | 23.0 °C | 830 MPa Show Material materials with Zugfestigkeit of 830 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K | |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1289 - 1478 °C Show Material materials with Schmelzpunkt of 1289 - 1478 °C | Typical for High Carbon Steel | |
Spezifische Wärmekapazität | 23.0 °C | 450 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 450 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 36 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 W/(m·K) | Typical for High Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Eisen | 98.3 - 98.8 % Show Material materials with Eisen of 98.3 - 98.8 % |
Kohlenstoff | 0.7 - 0.8 % Show Material materials with Kohlenstoff of 0.7 - 0.8 % |
Mangan | 0.5 - 0.8 % Show Material materials with Mangan of 0.5 - 0.8 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.05 % Show Material materials with Schwefel of 0 - 0.05 % |