Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 12.25-40 mm - Sheet: 75x8-85x18 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 280 [-] Show Supplier Material materials with Härte, Brinell of 280 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 3.8 - 4.5 % Show Supplier Material materials with Chrom of 3.8 - 4.5 % | |
Kohlenstoff | 1.2 - 1.35 % Show Supplier Material materials with Kohlenstoff of 1.2 - 1.35 % | |
Kupfer | 0.3 % Show Supplier Material materials with Kupfer of 0.3 % | max. |
Mangan | 0.2 - 0.35 % Show Supplier Material materials with Mangan of 0.2 - 0.35 % | |
Molybdän | 0.7 - 1.0 % Show Supplier Material materials with Molybdän of 0.7 - 1.0 % | |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.005 % Show Supplier Material materials with Schwefel of 0.005 % | max. |
Silizium | 0.15 - 0.3 % Show Supplier Material materials with Silizium of 0.15 - 0.3 % | |
Vanadium | 3.6 - 3.9 % Show Supplier Material materials with Vanadium of 3.6 - 3.9 % | |
Wolfram | 11.5 - 12.5 % Show Supplier Material materials with Wolfram of 11.5 - 12.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, industrial metrology, finishing and milling tools, cutting wheels, structural steels, reamers, turning and grooving steels for automatic work with good cooling | |
Processing history | Annealed |