Abmessung
Property | Value |
---|---|
Dimensions | 15x6-85x22 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 17.0 - 19.0 % Show Supplier Material materials with Chrom of 17.0 - 19.0 % | |
Kohlenstoff | 0.85 - 0.95 % Show Supplier Material materials with Kohlenstoff of 0.85 - 0.95 % | |
Mangan | 1.0 % Show Supplier Material materials with Mangan of 1.0 % | max. |
Molybdän | 0.9 - 1.3 % Show Supplier Material materials with Molybdän of 0.9 - 1.3 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1.00 % Show Supplier Material materials with Silizium of 1.00 % | max. |
Vanadium | 0.07 - 0.12 % Show Supplier Material materials with Vanadium of 0.07 - 0.12 % |
Technological properties
Property | ||
---|---|---|
Application areas | Apparatus engineering, shipbuilding, wear parts, perforated (Break) discs, balance pan and scale cutting, professional knives, high-quality cutting surgical instruments, rolling bearings, screw elements, spray nozzles | |
Processing history | Annealed |