Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 20-320 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 12 % Show Supplier Material materials with Dehnung of 12 % | min. |
Streckgrenze | 500.0 MPa Show Supplier Material materials with Streckgrenze of 500.0 MPa | min., RP02 |
Zugfestigkeit | 700.0 - 850.0 MPa Show Supplier Material materials with Zugfestigkeit of 700.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | max. |
Bor | 0.0015 % Show Supplier Material materials with Bor of 0.0015 % | |
Chrom | 10.0 - 11.5 % Show Supplier Material materials with Chrom of 10.0 - 11.5 % | |
Kohlenstoff | 0.17 - 0.23 % Show Supplier Material materials with Kohlenstoff of 0.17 - 0.23 % | max. |
Mangan | 0.4 - 0.9 % Show Supplier Material materials with Mangan of 0.4 - 0.9 % | |
Molybdän | 0.5 - 0.8 % Show Supplier Material materials with Molybdän of 0.5 - 0.8 % | |
Nickel | 0.2 - 0.6 % Show Supplier Material materials with Nickel of 0.2 - 0.6 % | |
Niobium | 0.25 - 0.55 % Show Supplier Material materials with Niobium of 0.25 - 0.55 % | |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. |
Stickstoff | 0.05 - 0.1 % Show Supplier Material materials with Stickstoff of 0.05 - 0.1 % | |
Vanadium | 0.1 - 0.3 % Show Supplier Material materials with Vanadium of 0.1 - 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant engineering, Mechanical Engineering, Power Generation, Components for high heat resistant pipelines, steam boiler and turbine construction and parts for the chemical industry and reactor technology | |
Processing history | Quenched and Tempered |