Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-125 mm |
Mechanisch
Property | Value |
---|---|
Zugfestigkeit | 510.0 - 690.0 MPa Show Supplier Material materials with Zugfestigkeit of 510.0 - 690.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.35 % Show Supplier Material materials with Aluminium of 0.35 % | max. |
Bor | 0.003 - 0.01 % Show Supplier Material materials with Bor of 0.003 - 0.01 % | |
Chrom | 13.5 - 16.0 % Show Supplier Material materials with Chrom of 13.5 - 16.0 % | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Molybdän | 1.0 - 1.8 % Show Supplier Material materials with Molybdän of 1.0 - 1.8 % | |
Nickel | 24.0 - 27.0 % Show Supplier Material materials with Nickel of 24.0 - 27.0 % | |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Titan | 1.9 - 2.3 % Show Supplier Material materials with Titan of 1.9 - 2.3 % | |
Vanadium | 0.1 - 0.5 % Show Supplier Material materials with Vanadium of 0.1 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering, Components for thermal power plants like valves, discs, housings, superheaters and steam line pipes | |
Processing history | Solution Annealed |