Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 20-250 mm |
Mechanisch
Property | Value |
---|---|
Zugfestigkeit | 620.0 - 850.0 MPa Show Supplier Material materials with Zugfestigkeit of 620.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 17.0 - 19.0 % Show Supplier Material materials with Chrom of 17.0 - 19.0 % | |
Kohlenstoff | 0.1 % Show Supplier Material materials with Kohlenstoff of 0.1 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Nickel | 9.0 - 12.0 % Show Supplier Material materials with Nickel of 9.0 - 12.0 % | |
Phosphor | 0.045 % Show Supplier Material materials with Phosphor of 0.045 % | max. |
Schwefel | 1.0 % Show Supplier Material materials with Schwefel of 1.0 % | max. |
Titan | 0.5 - 0.8 % Show Supplier Material materials with Titan of 0.5 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant engineering, Mechanical engineering, Power Generation, Fittings and accessories in boiler construction, Pipelines | |
Processing history | Quenched and Tempered |