Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 25-40 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Kohlenstoff | 0.15 % Show Supplier Material materials with Kohlenstoff of 0.15 % | max. |
Mangan | 0.3 - 0.8 % Show Supplier Material materials with Mangan of 0.3 - 0.8 % | |
Nickel | 4.75 - 5.25 % Show Supplier Material materials with Nickel of 4.75 - 5.25 % | |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | max. |
Silizium | 0.35 % Show Supplier Material materials with Silizium of 0.35 % | max. |
Vanadium | 0.05 % Show Supplier Material materials with Vanadium of 0.05 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Mechanical Engineering, Apparatus engineering | |
Processing history | Annealed |