Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 20-48 mm |
Mechanisch
Property | Value |
---|---|
Zugfestigkeit | 850.0 - 1250.0 MPa Show Supplier Material materials with Zugfestigkeit of 850.0 - 1250.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 3.0 - 5.0 % Show Supplier Material materials with Chrom of 3.0 - 5.0 % | |
Kohlenstoff | 0.3 - 0.5 % Show Supplier Material materials with Kohlenstoff of 0.3 - 0.5 % | |
Mangan | 18.0 - 20.0 % Show Supplier Material materials with Mangan of 18.0 - 20.0 % | |
Phosphor | 0.1 % Show Supplier Material materials with Phosphor of 0.1 % | max. |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | max. |
Silizium | 0.80 % Show Supplier Material materials with Silizium of 0.80 % | max. |
Stickstoff | 0.08 - 0.12 % Show Supplier Material materials with Stickstoff of 0.08 - 0.12 % |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, mechanical engineering, mechanically and thermally highly stressed components in shipbuilding, mechanical and vehicle engineering and in electrical engineering | |
Processing history | Strain Hardened |