Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 42-100 mm |
Mechanisch
Property | Value |
---|---|
Zugfestigkeit | 750.0 - 950.0 MPa Show Supplier Material materials with Zugfestigkeit of 750.0 - 950.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 3.0 - 5.0 % Show Supplier Material materials with Chrom of 3.0 - 5.0 % | |
Kohlenstoff | 0.3 - 0.5 % Show Supplier Material materials with Kohlenstoff of 0.3 - 0.5 % | |
Mangan | 17.0 - 19.0 % Show Supplier Material materials with Mangan of 17.0 - 19.0 % | |
Nickel | 1 % Show Supplier Material materials with Nickel of 1 % | max. |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Stickstoff | 0.1 % Show Supplier Material materials with Stickstoff of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, apparatus engineering, non-magnetisable components without special resistance to corrosion attacks | |
Processing history | Strain Hardened |