Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-270 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 35.0 - 40.0 % Show Supplier Material materials with Dehnung of 35.0 - 40.0 % | |
Härte, Brinell | 250 [-] Show Supplier Material materials with Härte, Brinell of 250 [-] | max. |
Streckgrenze | 280.0 MPa Show Supplier Material materials with Streckgrenze of 280.0 MPa | min., RP02 |
Zugfestigkeit | 580.0 - 800.0 MPa Show Supplier Material materials with Zugfestigkeit of 580.0 - 800.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 16.5 - 18.5 % Show Supplier Material materials with Chrom of 16.5 - 18.5 % | |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | max. |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | max. |
Molybdän | 2.5 - 3.0 % Show Supplier Material materials with Molybdän of 2.5 - 3.0 % | |
Nickel | 13.0 - 15.0 % Show Supplier Material materials with Nickel of 13.0 - 15.0 % | |
Phosphor | 0.045 % Show Supplier Material materials with Phosphor of 0.045 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Stickstoff | 0.15 - 0.25 % Show Supplier Material materials with Stickstoff of 0.15 - 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Metrology, mechanical engineering, connecting parts, shipbuilding | |
Corrosion properties | Resistant to intercrystalline corrosion, pitting and stress corrosion | |
Processing history | Solution Annealed |