Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 8-230 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 35 % Show Supplier Material materials with Dehnung of 35 % | min. |
Streckgrenze | 365.0 MPa Show Supplier Material materials with Streckgrenze of 365.0 MPa | min., RP02 |
Zugfestigkeit | 700.0 - 950.0 MPa Show Supplier Material materials with Zugfestigkeit of 700.0 - 950.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 20.0 - 21.5 % Show Supplier Material materials with Chrom of 20.0 - 21.5 % | |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | max. |
Mangan | 4.0 - 6.0 % Show Supplier Material materials with Mangan of 4.0 - 6.0 % | |
Molybdän | 3.0 - 3.5 % Show Supplier Material materials with Molybdän of 3.0 - 3.5 % | |
Nickel | 15.0 - 17.0 % Show Supplier Material materials with Nickel of 15.0 - 17.0 % | |
Niobium | 0.25 % Show Supplier Material materials with Niobium of 0.25 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Metrology, mechanical engineering, connecting parts, shipbuilding | |
Corrosion properties | Resistant to intercrystalline corrosion, pitting and stress corrosion | |
Processing history | Solution Annealed |