Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 16-36 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 17.0 - 19.0 % Show Supplier Material materials with Chrom of 17.0 - 19.0 % | |
Kohlenstoff | 0.1 % Show Supplier Material materials with Kohlenstoff of 0.1 % | max. |
Mangan | 7.5 - 9.5 % Show Supplier Material materials with Mangan of 7.5 - 9.5 % | |
Nickel | 4.5 - 6.5 % Show Supplier Material materials with Nickel of 4.5 - 6.5 % | |
Phosphor | 0.045 % Show Supplier Material materials with Phosphor of 0.045 % | max. |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Stickstoff | 0.1 - 0.2 % Show Supplier Material materials with Stickstoff of 0.1 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, connecting parts, components in shipbuilding and vehicle construction and for use in interior and exterior architecture and for pressure vessels down to -180 ° C | |
Processing history | Strain Hardened |