Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 16-50 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 21.5 - 24.5 % Show Supplier Material materials with Chrom of 21.5 - 24.5 % | |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | max. |
Mangan | 4.5 - 6.5 % Show Supplier Material materials with Mangan of 4.5 - 6.5 % | |
Molybdän | 2.8 - 3.4 % Show Supplier Material materials with Molybdän of 2.8 - 3.4 % | |
Nickel | 15.5 - 18.0 % Show Supplier Material materials with Nickel of 15.5 - 18.0 % | |
Niobium | 0.1 - 0.3 % Show Supplier Material materials with Niobium of 0.1 - 0.3 % | |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Stickstoff | 0.3 - 0.5 % Show Supplier Material materials with Stickstoff of 0.3 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Shipbuilding, electrical engineering, mechanical engineering | |
Corrosion properties | Resistant to intercrystalline corrosion, pitting and stress corrosion | |
Processing history | Solution Annealed |