Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6.5-310 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 16 % Show Supplier Material materials with Dehnung of 16 % | min. |
Streckgrenze | 750.0 MPa Show Supplier Material materials with Streckgrenze of 750.0 MPa | min., RP02 |
Zugfestigkeit | 900.0 - 1200.0 MPa Show Supplier Material materials with Zugfestigkeit of 900.0 - 1200.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.35 % Show Supplier Material materials with Aluminium of 0.35 % | max. |
Bor | 0.003 - 0.01 % Show Supplier Material materials with Bor of 0.003 - 0.01 % | |
Chrom | 13.5 - 16.0 % Show Supplier Material materials with Chrom of 13.5 - 16.0 % | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | max. |
Molybdän | 1.0 - 1.5 % Show Supplier Material materials with Molybdän of 1.0 - 1.5 % | |
Nickel | 24.0 - 27.0 % Show Supplier Material materials with Nickel of 24.0 - 27.0 % | |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Titan | 1.9 - 2.3 % Show Supplier Material materials with Titan of 1.9 - 2.3 % | |
Vanadium | 0.1 - 0.5 % Show Supplier Material materials with Vanadium of 0.1 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant construction, mechanical engineering, power generation | |
Processing history | Hardened |