Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6 mm -50 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 9 % Show Supplier Material materials with Dehnung of 9 % | min. |
Streckgrenze | 550.0 MPa Show Supplier Material materials with Streckgrenze of 550.0 MPa | min., RP02 |
Zugfestigkeit | 650.0 - 850.0 MPa Show Supplier Material materials with Zugfestigkeit of 650.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 11.5 - 13.5 % Show Supplier Material materials with Chrom of 11.5 - 13.5 % | |
Kohlenstoff | 0.08 - 0.15 % Show Supplier Material materials with Kohlenstoff of 0.08 - 0.15 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Nickel | 0.75 % Show Supplier Material materials with Nickel of 0.75 % | max. |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, mechanical engineering, petrochemistry, hydraulic engineering, petroleum industry, construction parts in water and steam and mildly acting agents of the food industry as well as rifle barrels | |
Processing history | Quenched and Tempered |