Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 8-80 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 20 % Show Supplier Material materials with Dehnung of 20 % | min. |
Härte, Brinell | 200 [-] Show Supplier Material materials with Härte, Brinell of 200 [-] | max. |
Streckgrenze | 240.0 MPa Show Supplier Material materials with Streckgrenze of 240.0 MPa | min., RP02 |
Zugfestigkeit | 400.0 - 630.0 MPa Show Supplier Material materials with Zugfestigkeit of 400.0 - 630.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 16.0 - 18.0 % Show Supplier Material materials with Chrom of 16.0 - 18.0 % | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Food technology, apparatus engineering, vehicle construction, plant engineering, parts for higher corrosion requirements with good deep-drawing and polishing properties, such as cutlery, sink linings, bumpers, wheel trims etc. | |
Processing history | Annealed |