Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-127 mm - Sheet: 50x40-70x40 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.1 % Show Supplier Material materials with Aluminium of 0.1 % | max. |
Kobalt | 9.3 % Show Supplier Material materials with Kobalt of 9.3 % | max. |
Kohlenstoff | 0.01 % Show Supplier Material materials with Kohlenstoff of 0.01 % | max. |
Mangan | 0.1 % Show Supplier Material materials with Mangan of 0.1 % | max. |
Molybdän | 5.0 % Show Supplier Material materials with Molybdän of 5.0 % | max. |
Nickel | 18.5 % Show Supplier Material materials with Nickel of 18.5 % | max. |
Silizium | 0.1 % Show Supplier Material materials with Silizium of 0.1 % | max. |
Titan | 0.75 % Show Supplier Material materials with Titan of 0.75 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Mechanical Engineering, Apparatus engineering | |
Processing history | Quenched and Tempered |