Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 16-52.15 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Zugfestigkeit | 770 MPa Show Supplier Material materials with Zugfestigkeit of 770 MPa | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 12.0 - 14.0 % Show Supplier Material materials with Chrom of 12.0 - 14.0 % | |
Kohlenstoff | 0.17 - 0.22 % Show Supplier Material materials with Kohlenstoff of 0.17 - 0.22 % | |
Mangan | 1.0 % Show Supplier Material materials with Mangan of 1.0 % | max. |
Molybdän | 0.9 - 1.3 % Show Supplier Material materials with Molybdän of 0.9 - 1.3 % | |
Nickel | 1.0 % Show Supplier Material materials with Nickel of 1.0 % | max. |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.02 % Show Supplier Material materials with Schwefel of 0.02 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant engineering, apparatus engineering, turbine blades, valve seats in superheated steam valves for temperatures up to approx. 500° C | |
Processing history | Quenched and Tempered |