Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-340 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 0.4 - 0.8 % Show Supplier Material materials with Chrom of 0.4 - 0.8 % | |
Kohlenstoff | 0.95 - 1.2 % Show Supplier Material materials with Kohlenstoff of 0.95 - 1.2 % | |
Mangan | 1.0 % Show Supplier Material materials with Mangan of 1.0 % | max. |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.04 % Show Supplier Material materials with Schwefel of 0.04 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Apparatus engineering, shipbuilding, ultra-hardenable and wear-resistant steel, especially suitable for smaller stainless steel ball bearings | |
Processing history | Annealed |