Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-325 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 15 % Show Supplier Material materials with Dehnung of 15 % | min. |
Streckgrenze | 650.0 MPa Show Supplier Material materials with Streckgrenze of 650.0 MPa | min., RP02 |
Zugfestigkeit | 780.0 - 980.0 MPa Show Supplier Material materials with Zugfestigkeit of 780.0 - 980.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 12.0 - 14.0 % Show Supplier Material materials with Chrom of 12.0 - 14.0 % | |
Kohlenstoff | 0.05 % Show Supplier Material materials with Kohlenstoff of 0.05 % | max. |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 0.3 - 0.7 % Show Supplier Material materials with Molybdän of 0.3 - 0.7 % | |
Nickel | 3.5 - 4.5 % Show Supplier Material materials with Nickel of 3.5 - 4.5 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.7 % Show Supplier Material materials with Silizium of 0.7 % | max. |
Stickstoff | 0.02 % Show Supplier Material materials with Stickstoff of 0.02 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant construction, power generation, pumps, armatures, compressors, turbine rotors, power plant components and reactor construction | |
Processing history | Quenched and Tempered |