Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 16-165.10 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 20 % Show Supplier Material materials with Dehnung of 20 % | min. |
Härte, Brinell | 310 [-] Show Supplier Material materials with Härte, Brinell of 310 [-] | max. |
Streckgrenze | 550.0 MPa Show Supplier Material materials with Streckgrenze of 550.0 MPa | min., RP02 |
Zugfestigkeit | 730.0 - 930.0 MPa Show Supplier Material materials with Zugfestigkeit of 730.0 - 930.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 24.0 - 26.0 % Show Supplier Material materials with Chrom of 24.0 - 26.0 % | |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Molybdän | 3.0 - 4.5 % Show Supplier Material materials with Molybdän of 3.0 - 4.5 % | |
Nickel | 6.0 - 8.0 % Show Supplier Material materials with Nickel of 6.0 - 8.0 % | |
Phosphor | 0.035 % Show Supplier Material materials with Phosphor of 0.035 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Stickstoff | 0.25 - 0.35 % Show Supplier Material materials with Stickstoff of 0.25 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, petrochemistry, apparatus engineering, chemistry, power plant construction, offshore, mechanical engineering, corrosion-resistant parts for the construction industry, mechanical engineering and general technical applications | |
Processing history | Solution Annealed |