Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-425 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 14 % Show Supplier Material materials with Dehnung of 14 % | min. |
Streckgrenze | 700.0 MPa Show Supplier Material materials with Streckgrenze of 700.0 MPa | min., RP02 |
Zugfestigkeit | 1.1 - 900.0 MPa Show Supplier Material materials with Zugfestigkeit of 1.1 - 900.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15.0 - 17.0 % Show Supplier Material materials with Chrom of 15.0 - 17.0 % | |
Kohlenstoff | 0.06 % Show Supplier Material materials with Kohlenstoff of 0.06 % | max. |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 0.8 - 1.5 % Show Supplier Material materials with Molybdän of 0.8 - 1.5 % | |
Nickel | 4.0 - 6.0 % Show Supplier Material materials with Nickel of 4.0 - 6.0 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.7 % Show Supplier Material materials with Silizium of 0.7 % | max. |
Stickstoff | 0.02 % Show Supplier Material materials with Stickstoff of 0.02 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Shipbuilding, offshore, plant construction, mechanical engineering, propeller shafts, axles, pump parts, centrifuge parts | |
Processing history | Quenched and Tempered |