Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 24-150 mm - Hexagonal Bar: 17- 41 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 35 % Show Supplier Material materials with Dehnung of 35 % | min. |
Streckgrenze | 220.0 MPa Show Supplier Material materials with Streckgrenze of 220.0 MPa | min., RP02 |
Zugfestigkeit | 530.0 - 730.0 MPa Show Supplier Material materials with Zugfestigkeit of 530.0 - 730.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 19.0 - 21.0 % Show Supplier Material materials with Chrom of 19.0 - 21.0 % | |
Kohlenstoff | 0.02 % Show Supplier Material materials with Kohlenstoff of 0.02 % | max. |
Kupfer | 1.2 - 2.0 % Show Supplier Material materials with Kupfer of 1.2 - 2.0 % | |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Molybdän | 4.0 - 5.0 % Show Supplier Material materials with Molybdän of 4.0 - 5.0 % | |
Nickel | 24.0 - 26.0 % Show Supplier Material materials with Nickel of 24.0 - 26.0 % | |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | max. |
Silizium | 0.7 % Show Supplier Material materials with Silizium of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant engineering, petrochemistry, apparatus engineering, chemistry | |
Corrosion properties | Particularly good resistance to highly corrosive media such as phosphorus, sulphur and hydrochloric acid media | |
Processing history | Solution Annealed |