Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 100 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 25 % Show Supplier Material materials with Dehnung of 25 % | min. |
Härte, Brinell | 192 [-] Show Supplier Material materials with Härte, Brinell of 192 [-] | max. |
Streckgrenze | 220.0 MPa Show Supplier Material materials with Streckgrenze of 220.0 MPa | min., RP02 |
Zugfestigkeit | 420.0 - 620.0 MPa Show Supplier Material materials with Zugfestigkeit of 420.0 - 620.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 17.0 - 19.0 % Show Supplier Material materials with Chrom of 17.0 - 19.0 % | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Nickel | 9.0 - 12.0 % Show Supplier Material materials with Nickel of 9.0 - 12.0 % | |
Niobium | 1.0 % Show Supplier Material materials with Niobium of 1.0 % | max. |
Phosphor | 0.045 % Show Supplier Material materials with Phosphor of 0.045 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, Apparatus engineering, Power Generation, Mechanical Engineering, Power plants, Plate girder and pipes in furnace construction, in apparatus engineering for air preheaters, Superheater suspensions, Annealing hoods, Rails, Barrels | |
Processing history | Annealed |