Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 12-65 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Zugfestigkeit | 1300 MPa Show Supplier Material materials with Zugfestigkeit of 1300 MPa | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 6.0 - 8.0 % Show Supplier Material materials with Chrom of 6.0 - 8.0 % | |
Kohlenstoff | 0.12 % Show Supplier Material materials with Kohlenstoff of 0.12 % | max. |
Kupfer | 0.5 - 1.0 % Show Supplier Material materials with Kupfer of 0.5 - 1.0 % | |
Mangan | 1.0 % Show Supplier Material materials with Mangan of 1.0 % | max. |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.5 - 1.0 % Show Supplier Material materials with Silizium of 0.5 - 1.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, Apparatus engineering, Tool making, Highly stressed exhaust valves in high-speed aircraft engines and racing engines | |
Processing history | Solution Annealed |