Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-80 mm |
Mechanisch
Property | Value |
---|---|
Zugfestigkeit | 500.0 - 750.0 MPa Show Supplier Material materials with Zugfestigkeit of 500.0 - 750.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 17.0 - 19.0 % Show Supplier Material materials with Chrom of 17.0 - 19.0 % | |
Kohlenstoff | 0.4 - 0.5 % Show Supplier Material materials with Kohlenstoff of 0.4 - 0.5 % | |
Mangan | 0.8 - 1.5 % Show Supplier Material materials with Mangan of 0.8 - 1.5 % | |
Nickel | 8.0 - 10.0 % Show Supplier Material materials with Nickel of 8.0 - 10.0 % | |
Phosphor | 0.045 % Show Supplier Material materials with Phosphor of 0.045 % | max. |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | max. |
Silizium | 2.0 - 3.0 % Show Supplier Material materials with Silizium of 2.0 - 3.0 % | |
Wolfram | 0.8 - 1.2 % Show Supplier Material materials with Wolfram of 0.8 - 1.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, Apparatus engineering, Power Generation, Power plants | |
Processing history | Solution Annealed |