Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-270 mm |
Mechanisch
Property | Value |
---|---|
Zugfestigkeit | 550.0 - 750.0 MPa Show Supplier Material materials with Zugfestigkeit of 550.0 - 750.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.04 % Show Supplier Material materials with Aluminium of 0.04 % | max. |
Chrom | 8.0 - 9.5 % Show Supplier Material materials with Chrom of 8.0 - 9.5 % | |
Kohlenstoff | 0.08 - 0.12 % Show Supplier Material materials with Kohlenstoff of 0.08 - 0.12 % | |
Mangan | 0.3 - 0.6 % Show Supplier Material materials with Mangan of 0.3 - 0.6 % | |
Molybdän | 0.85 - 1.05 % Show Supplier Material materials with Molybdän of 0.85 - 1.05 % | |
Nickel | 0.4 % Show Supplier Material materials with Nickel of 0.4 % | max. |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. |
Stickstoff | 0.03 - 0.07 % Show Supplier Material materials with Stickstoff of 0.03 - 0.07 % | |
Vanadium | 0.18 - 0.25 % Show Supplier Material materials with Vanadium of 0.18 - 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, Apparatus engineering, Ship building, Pressure vessels and steam boiler construction, Chemical industry | |
Processing history | Solution Annealed |