Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-500 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 12 % Show Supplier Material materials with Dehnung of 12 % | min. |
Härte, Brinell | 270.0 - 311.0 [-] Show Supplier Material materials with Härte, Brinell of 270.0 - 311.0 [-] | |
Streckgrenze | 750.0 MPa Show Supplier Material materials with Streckgrenze of 750.0 MPa | min., RP02 |
Zugfestigkeit | 900.0 - 1050.0 MPa Show Supplier Material materials with Zugfestigkeit of 900.0 - 1050.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Bor | 0.0015 - 0.005 % Show Supplier Material materials with Bor of 0.0015 - 0.005 % | |
Chrom | 10.0 - 18.0 % Show Supplier Material materials with Chrom of 10.0 - 18.0 % | |
Kohlenstoff | 0.04 % Show Supplier Material materials with Kohlenstoff of 0.04 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Molybdän | 2.0 - 3.0 % Show Supplier Material materials with Molybdän of 2.0 - 3.0 % | |
Nickel | 12.0 - 14.0 % Show Supplier Material materials with Nickel of 12.0 - 14.0 % | |
Phosphor | 0.035 % Show Supplier Material materials with Phosphor of 0.035 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.75 % Show Supplier Material materials with Silizium of 0.75 % | max. |
Stickstoff | 0.1 - 0.18 % Show Supplier Material materials with Stickstoff of 0.1 - 0.18 % |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, High temperature resistant components, Nuts, Screws | |
Processing history | Quenched and Tempered |