Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-525 mm - Hexagonal Bar: 13- 60 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 14 % Show Supplier Material materials with Dehnung of 14 % | min. |
Härte, Brinell | 245.0 - 285.0 [-] Show Supplier Material materials with Härte, Brinell of 245.0 - 285.0 [-] | |
Streckgrenze | 600.0 MPa Show Supplier Material materials with Streckgrenze of 600.0 MPa | min., RP02 |
Zugfestigkeit | 800.0 - 950.0 MPa Show Supplier Material materials with Zugfestigkeit of 800.0 - 950.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 10.0 - 12.5 % Show Supplier Material materials with Chrom of 10.0 - 12.5 % | |
Kohlenstoff | 0.17 - 0.23 % Show Supplier Material materials with Kohlenstoff of 0.17 - 0.23 % | |
Mangan | 0.3 - 1.0 % Show Supplier Material materials with Mangan of 0.3 - 1.0 % | |
Molybdän | 0.8 - 1.2 % Show Supplier Material materials with Molybdän of 0.8 - 1.2 % | |
Nickel | 0.3 - 0.8 % Show Supplier Material materials with Nickel of 0.3 - 0.8 % | |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | max. |
Vanadium | 0.2 - 0.35 % Show Supplier Material materials with Vanadium of 0.2 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant engineering, Mechanical Engineering, Power Generation, Components for reactor technology, chemical industry and turbines, steam boiler and pipeline construction | |
Processing history | Quenched and Tempered |