Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6.5-310 mm - Hexagonal Bar: 13- 60 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 16 % Show Supplier Material materials with Dehnung of 16 % | min. |
Härte, Brinell | 248.0 - 341.0 [-] Show Supplier Material materials with Härte, Brinell of 248.0 - 341.0 [-] | |
Streckgrenze | 600.0 MPa Show Supplier Material materials with Streckgrenze of 600.0 MPa | min., RP02 |
Zugfestigkeit | 900.0 - 1150.0 MPa Show Supplier Material materials with Zugfestigkeit of 900.0 - 1150.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15.0 - 17.0 % Show Supplier Material materials with Chrom of 15.0 - 17.0 % | |
Kohlenstoff | 0.04 - 0.1 % Show Supplier Material materials with Kohlenstoff of 0.04 - 0.1 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Nickel | 24.0 - 27.0 % Show Supplier Material materials with Nickel of 24.0 - 27.0 % | |
Phosphor | 0.035 % Show Supplier Material materials with Phosphor of 0.035 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.3 - 0.6 % Show Supplier Material materials with Silizium of 0.3 - 0.6 % | |
Titan | 0.0001 % Show Supplier Material materials with Titan of 0.0001 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant engineering, Mechanical Engineering, Power Generation, Parts for gas turbines and engines like runners, discs, shafts, screws, extension rings, fittings, housings | |
Processing history | Hardened |