Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 14.52-115 mm - Hexagonal Bar: 24- 55 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 17 % Show Supplier Material materials with Dehnung of 17 % | min. |
Härte, Brinell | 200.0 - 260.0 [-] Show Supplier Material materials with Härte, Brinell of 200.0 - 260.0 [-] | |
Streckgrenze | 500.0 MPa Show Supplier Material materials with Streckgrenze of 500.0 MPa | min., RP02 |
Zugfestigkeit | 650.0 - 850.0 MPa Show Supplier Material materials with Zugfestigkeit of 650.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.35 % Show Supplier Material materials with Aluminium of 0.35 % | max. |
Bor | 0.003 - 0.01 % Show Supplier Material materials with Bor of 0.003 - 0.01 % | |
Chrom | 13.5 - 16.0 % Show Supplier Material materials with Chrom of 13.5 - 16.0 % | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Molybdän | 1.0 - 1.8 % Show Supplier Material materials with Molybdän of 1.0 - 1.8 % | |
Nickel | 24.0 - 27.0 % Show Supplier Material materials with Nickel of 24.0 - 27.0 % | |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Titan | 1.9 - 2.3 % Show Supplier Material materials with Titan of 1.9 - 2.3 % | |
Vanadium | 0.1 - 0.5 % Show Supplier Material materials with Vanadium of 0.1 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power Generation, Connecting parts, Steam and gas turbine components like parts for mechanical systems, furnace construction, chemical and petrochemical industry and reactor technology | |
Processing history | Strain Hardened |