Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10.68-100 mm |
Mechanisch
Property | Value |
---|---|
Zugfestigkeit | 530.0 - 710.0 MPa Show Supplier Material materials with Zugfestigkeit of 530.0 - 710.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Bor | 0.05 - 0.1 % Show Supplier Material materials with Bor of 0.05 - 0.1 % | |
Chrom | 13.5 - 17.5 % Show Supplier Material materials with Chrom of 13.5 - 17.5 % | |
Kohlenstoff | 0.04 - 0.1 % Show Supplier Material materials with Kohlenstoff of 0.04 - 0.1 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 1.6 - 2.0 % Show Supplier Material materials with Molybdän of 1.6 - 2.0 % | |
Nickel | 15.5 - 17.5 % Show Supplier Material materials with Nickel of 15.5 - 17.5 % | |
Niobium | 1.2 % Show Supplier Material materials with Niobium of 1.2 % | max. |
Phosphor | 0.045 % Show Supplier Material materials with Phosphor of 0.045 % | max. |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | max. |
Silizium | 0.3 - 0.6 % Show Supplier Material materials with Silizium of 0.3 - 0.6 % |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, Mechanical Engineering, Components in machines and apparatus engineering, Cooling machine parts and similarly claimed parts for temperatures to -150°C | |
Processing history | Quenched and Tempered |