Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 24.83-30.5 mm |
Mechanisch
Property | Value |
---|---|
Zugfestigkeit | 1040.0 - 1240.0 MPa Show Supplier Material materials with Zugfestigkeit of 1040.0 - 1240.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 1.8 - 2.3 % Show Supplier Material materials with Chrom of 1.8 - 2.3 % | |
Kohlenstoff | 0.26 - 0.34 % Show Supplier Material materials with Kohlenstoff of 0.26 - 0.34 % | |
Mangan | 0.3 - 0.6 % Show Supplier Material materials with Mangan of 0.3 - 0.6 % | |
Molybdän | 0.3 - 0.65 % Show Supplier Material materials with Molybdän of 0.3 - 0.65 % | |
Nickel | 1.8 - 2.3 % Show Supplier Material materials with Nickel of 1.8 - 2.3 % | |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | max. |
Silizium | 0.15 - 0.4 % Show Supplier Material materials with Silizium of 0.15 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, Mechanical Engineering | |
Processing history | Quenched and Tempered |