Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 14.52-52.14 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 22 % Show Supplier Material materials with Dehnung of 22 % | min. |
Streckgrenze | 690.0 MPa Show Supplier Material materials with Streckgrenze of 690.0 MPa | min., RP02 |
Zugfestigkeit | 830.0 - 1080.0 MPa Show Supplier Material materials with Zugfestigkeit of 830.0 - 1080.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 - 0.05 % Show Supplier Material materials with Aluminium of 0.02 - 0.05 % | |
Chrom | 1.2 - 1.5 % Show Supplier Material materials with Chrom of 1.2 - 1.5 % | |
Kohlenstoff | 0.18 - 0.25 % Show Supplier Material materials with Kohlenstoff of 0.18 - 0.25 % | |
Mangan | 0.3 - 0.5 % Show Supplier Material materials with Mangan of 0.3 - 0.5 % | |
Molybdän | 0.25 - 0.5 % Show Supplier Material materials with Molybdän of 0.25 - 0.5 % | |
Nickel | 3.4 - 4.0 % Show Supplier Material materials with Nickel of 3.4 - 4.0 % | |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | max. |
Silizium | 0.15 - 0.4 % Show Supplier Material materials with Silizium of 0.15 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts | |
Processing history | Strain Hardened |