Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 14.52-120 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 - 0.05 % Show Supplier Material materials with Aluminium of 0.02 - 0.05 % | |
Chrom | 1.2 - 1.7 % Show Supplier Material materials with Chrom of 1.2 - 1.7 % | |
Kohlenstoff | 0.25 - 0.3 % Show Supplier Material materials with Kohlenstoff of 0.25 - 0.3 % | |
Mangan | 0.2 - 0.5 % Show Supplier Material materials with Mangan of 0.2 - 0.5 % | |
Molybdän | 0.35 - 0.55 % Show Supplier Material materials with Molybdän of 0.35 - 0.55 % | |
Nickel | 3.3 - 3.8 % Show Supplier Material materials with Nickel of 3.3 - 3.8 % | |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % | max. |
Vanadium | 0.12 % Show Supplier Material materials with Vanadium of 0.12 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering | |
Processing history | Quenched and Tempered |