Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 14-75 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Cerium | 0.45 % Show Supplier Material materials with Cerium of 0.45 % | max. |
Kohlenstoff | 0.2 % Show Supplier Material materials with Kohlenstoff of 0.2 % | max. |
Kupfer | 0.55 % Show Supplier Material materials with Kupfer of 0.55 % | max. |
Mangan | 1.6 % Show Supplier Material materials with Mangan of 1.6 % | max. |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | |
Silizium | 0.55 % Show Supplier Material materials with Silizium of 0.55 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering | |
Processing history | Annealed and Forged |